Galvanic corrosion caused by dissimilar metals and acidic water is becoming a major concern. In the past year we have had several companies contact us for an alternative for their aluminum manifolds used for the distribution of water in their molds. Many have told us horror stories of threads failing and fittings flying out of the manifold creating a safety hazard in the work place. Affordable custom manifold has developed a stainless steel manifold that doesn’t react to the brass fittings and can handle the harsh conditions caused by acidic water. The manifolds are competitively priced and are custom built to meet your requirements
Check out Affordable Custom Manifolds website at WWW.acmgr.net